Technical Parameters
product introduction:
Container desiccant is a special solution for container cargo damp problem, can effectively absorb excess water vapor to create a dry environment for the inside of container, and thus to ensure the safe transport of products to prevent product packaging from damage, mildew, corrosion and so on.
During container shipping and storage, containers often experience high humidity climate in the ocean and strong day and night temperature difference between the changes in humidity during the day up to 98%, the high temperature air which sealed in the container is rich in water vapor, it reaches saturation at night due to the temperature drop in water vapor, the water vapor inside the container will condense into water droplets, this liquid water will have a serious impact on goods inside of the container or the outside packaging of goods, and then causing mold, bacteria and damage to the goods, if the water coagulation occurs on the metal surface, it will lead to rust.
Applications:
Agricultural products, wood products, textiles, leather products, food packaging, canned food, pet food, furniture, household goods, color box packaging, electronic appliances, medical equipment, hardware products, military products, precision instruments, machinery and equipment.
Container packaging and usage:
Container model |
Minimum usage |
||
CODC-91-10 |
CODB-91-10 |
CODC-91-14 |
|
20GP |
6 |
6 |
4 |
40GP |
12 |
12 |
8 |
40HQ |
14 |
14 |
10 |
Notes:
1.For the humidity of the wood flooring in the container is more than 20%, a dry bar should be added for every 1.5% humidity. Linen or cotton mats, each container should add 1 more container desiccant. For the humidity of the furniture itself is in 18% or more, more than 1% of the humidity is required to put one more dry bar. Rattan, palm, seaweed and other materials which may be made of any moisture-containing products, each container needs to add two additional drying rods.
2.If the card board needs to be used in the container and card board humidity is more than 18% one more dry rod should be added as per 1.5% increase.